Magnetics Inc

Magnetics Inc

  • 0078083A7

    01001012

    Composition 6.5 SiFe alloy Saturation Flux Density 1.6 Tesla Typical Core Loss (50kHz,100mT) 650 mW/cm3 Curie Temperature 700˚C Operating Temperature Range -30˚C to 200˚

    $12.00
  • C058380A2

    01001013

    High Saturation (1.5 T) Lower core loss than Iron Powder or Laminated Silicon Lower cost than MPP material Best DC Bias Very high Curie temperature Stable performance